Elongation at break of membranes made of pure CTA or comprising either raw or acetylated lignins.

Synthesis conditions Elongation at break (%) of membranes:
With raw lignins With acetylated lignins
T (°C) HR (%) CTA MKL MOL MHL MAKL MAOL MAHL
35 10 7.81 4.865 7.50 6.03 7.34 5.55 5.41
35 70 9.20 6.64 9.26 8.91 6.83 12.12 4.77
45 30 7.07 6.66 10.36 8.33 4.68 9.44 4.94
45 70 8.715 6.575 5.76 8.09 6.85 5.36 5.60
55 10 7.05 3.745 6.05 3.74 6.045 7.00 4.90