. 2012 Jul 31;13(4):043001. doi: 10.1088/1468-6996/13/4/043001

Table 3.

Microstructure and properties of TiAlCrN-based coatings [ 17, 242].

Coating Microstructure Microhardness (GPa)
Maximum impact depth (nm;150 mN load) Residual stress (GPa) Weight gain, TG (%) after oxidation in air (0.5 h, 1000 °C) DTA (μV;at 1000 °C)
25 °C 500 °C
TiAl55CrSiYN Nanocrystalline monolayer 29.9+3.5 19.2+2.8 6155+359 −0.490 0.015 27.96
TiAl55CrSiYN/TiAlCrN Nanocrystalline multilayer 30.0+4.8 27.4+4.1 5901+207 −0.520 −0.020 −41.74