Skip to main content
. 2010 Nov 29;11(5):055002. doi: 10.1088/1468-6996/11/5/055002

Figure 4.

Figure 4.

Photodegradation of MB using photocatalytic paper with ZnO nanorods of different dimensions (samples 1 and 2). Sample 1 with thicker and longer nanorods showed higher photoreactivity (93% degradation after 120 min) than sample 2 (89% degradation after 120 min). The control sample of paper without ZnO nanorods showed 30% degradation in 120 min. Light intensity at the sample: 963 Wm–2, error bar: 5%.