(A) Phase separation of PLGA and PFOB in the absence of Pluronic F-68 results in nonporous shells. (B) Fluorescent microscopy confirms the solid nature of PLGA shell in the absence of F-68. (C) Freeze-drying results in persistence of core–shell particles with PFOB-filled cores as PFOB is not permeable through the PLGA shell.