. 2008 Jul 7;9(2):024401. doi: 10.1088/1468-6996/9/2/024401

Figure 2.

Figure 2

Changes in ratio of molecular weights (Mn, t/Mn, 0) of ZiPP and ZiPP/MiPP during thermal oxidative degradation at 130 °C; Mn, t and Mn, 0 are number average molecular weights after and before thermal oxidative degradation, respectively.