Skip to main content
. 2016 Mar 9;17(1):45–57. doi: 10.1080/14686996.2016.1140306

Figure 3.

Figure 3.

(a) Polarization hysteresis loop before fatigue treatment; (b) relative dielectric constant ɛ r and dielectric loss tangent loops; (c) piezoelectric coefficient d 33 of 200 nm thick (001)- and (110)-oriented PMN-PT films on CeO2/YSZ buffered Si(001) substrate, using SRO electrodes.