Figure 3.

Plots of (a) tan δ vs temperature and (b) storage modulus vs temperature for a series of azide monomers (AZ-(1–4)) with a single alkyne monomer (AL-1). All resins were composed 2 mol % CuCl2[PMDETA] and 4 mol % DMPA and were cured with 10 mW/cm2 UV light. Representative curves are presented as the third cycle in the DMA.