Figure 4.
Effect of water-aging time on self-healing of composite containing 7.5% microcapsules. (A) Virgin and healed fracture toughness, and (B) self-healing efficacy (mean ± sd; n = 6). The cured composite specimens were water-aged for 1 d to 6 months (with 6 specimens for each time period), and then fractured to measure KIC-virgin. They were then healed in a humidor in air for 1 d and then re-fractured to measure KIC-healed. In (A), values with dissimilar letters are significantly different from each other (p < 0.05). In (B), all values are statistically similar (p > 0.1).