Skip to main content
. Author manuscript; available in PMC: 2017 Feb 1.
Published in final edited form as: Dent Mater. 2015 Dec 29;32(2):294–304. doi: 10.1016/j.dental.2015.11.014

Figure 3.

Figure 3

DSC diagram of microcapsules containing TEGDMA-DHEPT healing liquid inside PUF shells. The exothermic peak at 162 °C was due to polymerization of TEGDMA by the high temperature. The endothermic valley at 307 °C was related to PUF shell decomposition. These microcapsules were stable up to 150 °C, indicating suitability for use at temperatures in vivo in dentistry.