Skip to main content
. 2016 Nov 25;6:37503. doi: 10.1038/srep37503

Figure 3.

Figure 3

In-plane (black) and out-of-plane (red) magnetic hysteresis loops of as-grown, 350 °C, and 400 °C-annealed Stack B samples, where the CoO thickness was fixed at 0.5 nm and the oxygen content was varied by controlling the flow rate to (a) 1.5 sccm, (b) 3.5 sccm, and (c) 5 sccm.