In-plane (black) and out-of-plane (red) magnetic hysteresis loops of as-grown, 350 °C, and 400 °C-annealed Stack B samples, where the fixed oxygen content was 5 sccm and the CoO thickness was (a) tCoO = 0.3 nm, (b) tCoO = 0.5 nm, (c) tCoO = 0.7 nm, and (d) tCoO = 1.0 nm.