Skip to main content
. 2016 Nov 25;6:37503. doi: 10.1038/srep37503

Figure 6.

Figure 6

HR-XRD patterns of as-grown, 350 °C and 400 °C post-annealed Stack B samples as a function of oxygen content with a fixed CoO thickness of 0.5 nm: (a) 1.5 sccm, (b) 3.5 sccm, and (c) 5 sccm.