Figure 4.

Figure 4

(a) The as-grown type B WS2 film on 2-inch sapphire wafer; (b) separated polystyrene polymer-coated WS2 film floated on water; (c) 2-inch WS2 thin film transferred to a four inch SiO2/Si wafer without observable wrinkles, cracks and polymer residues; and (d) optical image of WS2 after being transferred to the SiO2.