Skip to main content
. 2016 Dec 9;11(12):e0167084. doi: 10.1371/journal.pone.0167084

Fig 9. (a) The saturated ferroelectric polarization hysteresis (P-E) loop, and (b) a plot of current as a function of voltage (I-V curve) of SrFe12O19 ceramic.

Fig 9

The ceramic has been sintered at 1150°C for 1 hour and subsequently annealed at 800°C in pure oxygen for a total duration of 9 hours in 3 steps wise. The measurement was made at a frequency of 33Hz and room temperature (300K).