Film name Thickness (μm) [E] (kPa) TS (kPa) S (%) t B (min) t R (min)
CD 0.0 1451 ± 74 58 ± 46 18 ± 2 962 ± 24 60 ± 3 30 ± 4
CD 0.5 1431 ± 90 228 ± 40 39 ± 4 1102 ± 40 70 ± 7 50 ± 2
CD 1.0 1258 ± 68 239 ±30 64 ± 9 1293 ± 62 60 ± 5 25 ± 3
CD 1.5 901 ± 74 507 ± 80 94 ± 11 1474 ± 46 40 ± 6 35 ± 7
AGCa 0.04 592 ± 97 1010 ± 246 27 ± 8 347 ± 24 45 ± 5 55 ± 6
AGCa 0.08 351 ± 143 1915 ± 220 67 ± 7 335 ± 56 30 ± 3 35 ± 1
AGCa 0.12 677 ± 68 2086 ± 400 107 ± 13 237 ± 28 35 ± 1 35 ± 3