Skip to main content
. 2016 Dec 16;6:39192. doi: 10.1038/srep39192

Table 1. Poly(NIPAM) samples produced by RAFT polymerisation for this study.

Polymer CTA DPNMR Inline graphic/kDa Inline graphic/kDa Đ Other Information
P1a 1 50 6.0 5.3 1.14
P1b 1 97 11.3 10.4 1.14
P1c 1 196 22.5 20.0 1.18
P2 2 98 11.1 9.6 1.10 >99% PFP incorporation
P3 3 78 8.8 7.8 1.10 80–95% NHS incorporation
P4a 1 50 6.0 5.7 1.17 47% free thiol
P4b 1 97 11.3 11.7 1.23 37% free thiol
P4c 1 196 22.5 21.4 1.30 27% free thiol
P5 4 61 7.3 6.9 1.16
P6 9 105 12.5 11.5 1.05 98% PFP incorporation
P7 9 105 12.5 13.1 1.04 53% Tz incorporation
P8 145 16.4 1.12 >99% Nb incorporation

DMF was used as the SEC eluent in all cases, with poly(methyl methacrylate) standards. DP = Degree of polymerisation.