. 2016 Nov 16;9(4):213–221. doi: 10.11138/orl/2016.9.4.213

Table 5.

Statistical analysis of the tensile force before and after cyclic loading.

Groups of specimen Before cyclic loading (n=5) After cyclic loading (n=10)
Group A 6.91 ± 7.12 62.78 ± 14.16
Group B 67.20 ± 13.12 172.36 ± 45.49
Group C 50.28 ± 9.07 183.68 ± 46.59