Skip to main content
. Author manuscript; available in PMC: 2017 Jan 3.
Published in final edited form as: J Biomed Mater Res A. 2016 Feb 1;104(4):1017–1029. doi: 10.1002/jbm.a.35614

FIGURE 5.

FIGURE 5

FTIR spectra of PCL/gelatin composite electrospun scaffolds with and without crater-like structures. FTIR peaks of (A) PCL/gelatin (100/0, 75/25, 50/50, and 25/75) scaffolds without crater-like structures and (B) with crater-like structures at 2 hours after degradation. (C) The scaffolds without crater-like structures and (D) with crater-like structures at 7 days after degradation.