. 2016 Sep 9;6(9):168. doi: 10.3390/nano6090168

Figure 6.

Figure 6

Optical micrographs of silver film containing controlled cracks and wrinkles under various strain of (a) 0%, (b) 2.2%, (c) 6.1%, and (d) 7.4%.