Figure 2.

Figure 2

TEM-HAADF image of (a) 450 °C, and (b) 750 °C annealed Fe2O3/Al2O3. In Fe2O3/Al2O3 sample, Fe2O3 nanoparticles are uniformly distributed (a,b), and as annealing temperature increased from (a) 450 °C to (b) 750 °C, the particle size of Fe2O3 increased.