Skip to main content
. 2016 Nov 14;7:1709–1717. doi: 10.3762/bjnano.7.163

Figure 4.

Figure 4

XRD pattern for Ni NWs in alumina template with HPA of 65 μm and a current density of 3 mA·cm−2, deposition duration 120 min.