Figure 6

Normalized signal change at a constant angle in response to binding of DEP to rGO-modified nanohole arrays (D/P = 0.43) covering a concentration range from 0.05 to 5 µM. For comparison the response of a continuous gold film modified with rGO is shown. Error bars indicate S/N. Data were fitted with the Langmuir equation (Equation 1).