Figure 5.
Porous structure and drug release behavior of the hybrid NCs. (a) N2 adsorption-desorption isotherm and (b) pore diameter distribution of Fe3O4@CDs@mSiO2@PTX@mSiO2 NCs. (c) HPLC analysis of initial PTX solution and residual PTX solution from the preparation of Fe3O4@CDs@mSiO2@PTX@mSiO2 NCs. (d) Release profiles of PTX from Fe3O4@CDs@mSiO2@PTX@mSiO2 NCs in PBS at 37°C, with or without of irradiation of NIR light. NIR was irradiated at 1.5 W cm−2 for 5 min each at predefined time points (6, 22, and 32 h). The inset in (d) is a schematic illustration of the release of PTX from Fe3O4@CDs@mSiO2@PTX@mSiO2 NCs.