Skip to main content
. 2016 Dec 16;121(2):1171–1181. doi: 10.1021/acs.jpcc.6b10363

Table 1. Accessible Surface Area (ASA), Accessible Volume (AV), Largest Included Sphere (DI), Largest Free Sphere (DF), Open Metal Site Volumetric Density (ρMg), and Open Metal Site Weight Percent of Two Frameworks: Mg2(DHFUMA) vs Mg2(DOBDC).

  ASA AV DI DF ρMg wt % Mg
ligand [m2/g] [cm3/g] [Å] [Å] [Mg/Å3] [%]
DOBDC 1782 0.350 11.8 11.1 0.0044 20.0
DHFUMA 1043 0.095 7.6 6.3 0.0084 25.2