Skip to main content
. 2016 Dec;16(4):369–376.

Table 2.

Biomechanical characteristics of sham-vehicle, sham-selenate, FPI-vehicle and FPI-selenate femoral samples. There were no differences in any measured mechanical properties between any groups. Values are mean ± SEM.

SHAM + VEH (n=15) SHAM + SS (n=15) FPI + VEH (n=14) FPI + SS (n=14)
Peak force (N) 222±6 221±7 230±10.7 225±11
Stiffness (x 104 Nm2) 29.5±1.0 30.1±1.1 29.7±1.0 29.2±1.1
Cross sectional area (x 10-6 µm2) 6.8±0.2 6.8±0.2 6.2±0.6 6.8±0.3
Ultimate bending stress (x 107 Nm-2) 6.9±0.2 6.8±0.2 6.8±0.2 7.0±0.3
Bending modulus (x 109 Nm-2) 3.4±0.2 3.4±0.2 3.2±0.2 3.4±0.1