Skip to main content
. 2017 Jan 24;5:7. doi: 10.1186/s40349-017-0085-z

Fig. 1.

Fig. 1

Nanosight results for OFP-filled PCCAs (N = 3 vials). The mean particle size (±SD) was found to be 140 ± 10 nm and the average concentration (±SD) was 1.7 ± 0.1 × 1012 particles/mL