Skip to main content
. 2017 Jan 27;7:41336. doi: 10.1038/srep41336

Figure 5.

Figure 5

(a) Fractional resistance changes of the Ag and Al2O3/Ag nanowire electrodes under 2.5% applied strain as a function of the number of bending cycles: up to (a) 1,200 and (b) 500,000 cycles. The corresponding value for the reference ITO sample is also included in (a).