Table 1. Values of the maximum sensitivity and relative sensitivity of different Er3+ and Er3+/Yb3+ co-doped materials using the FIR method to obtain the green emissions of the Er3+.

Doped materials Smax(10−3 K−1) SR§ (% K−1) Tmax (°C) ΔT (°C) λexc(nm) Ref.
Er3+/Yb3+:tellurite glass 8.9 0.53 200 5–200 980 This work
Er3+:fluorotellurite glass 5.4 0.35 267 27–267 800 28
Er3+/Yb3+:chalcogenide glass 5.2 0.38 220 20–220 1060 26
Er3+/Yb3+:Al2O3 nanoparticle 5.1 0.40 218 22–700 978 9
Er3+/Yb3+:germanate tellurite glass 3.6 0.39 220 20–220 976 46
Er3+/Yb3+:silicate glass 3.3 0.63 23 23–450 978 44
Er3+:fluoroindate glass 2.8 0.55 152 −150–152 980 48
Er3+:oxyfluoride glass 2.7 0.41 240 −23–177 980 47
Er3+:PbO-Ga2O3-SiO2 glass 2.6 0.24 317 23–377 980 10
Er3+/Yb3+:TeO2–WO3 glass 2.6 0.20 417 27–417 980 27
Er3+/Yb3+:fluorophosphate glass 1.5 0.71 6 −196–227 980 49
Er3+:fluorozirconate glass 0.6 0.58 27 −123–577 976 45

The temperature range, excitation wavelength, and temperature for the maximum sensitivity values are also included. §SR values were extracted by the authors from the references data (WebPlotDigitizer).