Skip to main content
. 2017 Jan 31;7:41891. doi: 10.1038/srep41891

Table 1. The water contact angle (WCA) on graphene nanosheets before and after plasma treatment.

Plasma treatment time (s) 0 1 2 3 6 9 12
WCA (°) 89.5 74.7 70.4 63.4 58.4 52.9 45.4