Skip to main content
. Author manuscript; available in PMC: 2017 Dec 23.
Published in final edited form as: Angew Chem Int Ed Engl. 2016 Nov 24;55(52):16039–16043. doi: 10.1002/anie.201609043

Figure 1.

Figure 1

Characterization of glutathione-coated Au-Ag alloy nanoparticles (GS-Au/AgNPs). A) Typical transmission electron microscopy (TEM) image of GS-Au/AgNPs. B) A core size of 2.6±0.2 nm, and dynamic light scattering analysis showing a hydrodynamic diameter (HD) of 3.1±0.3 nm in aqueous solution. C) STEM and EOS mapping images of the GS-Au/AgNPs with a Au/Ag molar ratio of 1.4. scale bar=2 nm