Skip to main content
. 2017 Feb 6;12:89. doi: 10.1186/s11671-017-1875-5

Table 2.

Summary of the experimental results of three different systems studied in this work

System Sample SSA (m2/g) f R d A (nm) d R (nm) R 0/R at 300 °C, 3000 ppm H2 Figure
Undoped TiO2 As-obtained 67.7 0.07 20 16 4 1
Annealed at 700 °C 0.75 37 57 10
TiO2:5 at.% Cr Mostly anatase 126.6 0.16 9 8 3 2
Mostly rutile 102.9 0.77 12 11 12
TiO2-SnO2 TiO2 57 0.05 25 9 2 3
10% SnO2 60 0.73 28 14 8.5