Detection Mechanism | Material | Optical Fibre Configuration | Analyte | Dynamic Range | Sensitivity | Response Time | Ref. |
---|---|---|---|---|---|---|---|
MZI | GO | PCF MZI | RI | 1.33–1.37 | 212 nm/RIU 130 dB/RIU | - | [70] |
MZI | G | PCF MZI | RI | 1.38–1.43 | 17.5 dB/RIU | - | [69] |
MZI | G | 2-arms MZI | Ammonia | 40–360 ppm | ~6 pm/ppm | 0.4 s | [68] |
SPR | Cu + rGO/PMMA | Uncladded MMF | Ammonia | 10–100 ppm | ~1 nm/ppm | - | [94] |
SPR | Ag + rGO/CNT/PMMA | Uncladded MMF | Methane | 10–100 ppm | 0.33 nm/ppm | - | [93] |
LSPR | GOE-Au NPs | Uncladded MMF | RI | 1.34–1.38 | 2.288 ΔA/RIU | - | [97] |
LSPR | GOE-Ag NPs | Uncladded MMF | RI | 1.34–1.38 | 0.940 ΔA/RIU | - | [98] |
Bragg wavelength | rGO | Etched FBG | Strain and Temperature | - | 5.5 pm/μє 33 pm/°C | - | [113] |
Bragg wavelength | rGO | Etched FBG | NO2 | 0.5–3 ppm | - | 6 to 20 min | [143] |
Bragg wavelength | APBA-rGO | Etched FBG | Glucose | 1 nM–10 mM | [109] | ||
Bragg wavelength | Dendrimers-GO | Etched FBG | Lectin Con A | 500 pM | - | - | [114] |
Bragg wavelength | antiCRP-GO | Etched FBG | CR Protein | 0.01–100 mg/L | 6.3 pm/CRP magnitude order | - | [111] |
Bragg wavelength | p-doped G | D-shaped polymer FBG | Erythrocyte | - | 1 pm/ppm | - | [144] |
Bragg power at 1557 nm | GO | Tilted FBG | Relative Humidity | 10%–80%HR | 0.129 dB/%RH | - | [115] |
Bragg wavelength | PMMA-G | MFBG | Ammonia | 0–100 ppm | 6 pm/ppm | - | [116] |
Absorption | GO | Tapered MMF | Aqueous Ethanol | - | - | 20–30 s | [129] |
Reflectance | GO | Tapered MMF | Aqueous Ethanol | 5%–80% | 0.02–0.0275 ∆R/∆C 1 | 19–25 s | [130] |
Absorption | GO | Tapered MMF | Aqueous Ethanol | 5%–40% | 0.829 ∆A/∆C 1 | 15–40 s | [127,128] |
Absorption | GO | U-bent MMF | Aqueous Ethanol | 5%–100% | 0.44–0.0925 ∆A/∆C 1 | 1–2 s | [131] |
Absorption | GO, rGO | CRMMF | Ethanol, methanol, ammonia | 0–500 ppm | 0.26, 0.2 and 0.32 counts/ppm | - | [132] |
Absorption | Graphene/PANI | Side-polished MMPF | ammonia | 0%–1% vol. | 4.1 ∆A/∆vol. 1 | 24–71.8 s | [145] |
Absorption | GO-rGO | POF | VOCs | - | - | - | [133] |
Absorption | rGO | Side-polished SMF | Temperature | −7.8–77 °C | 0.134 dB·°C−1 | - | [123] |
Absorption | rGO | Tapered SMF | Temperature | 30–80 °C | 0.1018 dB·°C−1 | - | [122] |
Absorption | rGO | Side-polished SMF | Humidity | 70%–95% RH | 0.31 dB/%RH | 0.13% RH/s | [126] |
Absorption | GO | Tapered POF | Glucose | 1%–40% vol. | - | - | [134] |
Absorption | Graphene | Tapered MMF | DS-DNA | 5–400 μM | 0.0475 ∆A/μM | <30 s | [135] |
Absorption | GO | HB fibre | UV light | 2–4 mW | ~0.12 ∆A/mW | - | [124] |
Absorption | MB-rGO | Tapered SMF | UV light | 0.03–12.77 mW | ~0.235 dB/mW | - | [125] |
Fluorescence | prGO | Etched MMF | Cd2+ ions, DA, ssDNA | - | - | - | [142] |