Skip to main content
. 2016 Feb 15;6(2):32. doi: 10.3390/nano6020032

Figure 5.

Figure 5

(a) Time-resolved DAP PL decay of Ga2O3 NCs containing different amounts of surface-bound TGA without CdSe/CdS NCs. TGA equivalents and absolute concentrations (in parentheses) in Ga2O3 NC suspensions are indicated in the graph (aqua blue trace (0.84 mM) represents TGA concentration for the highest acceptor to donor ratio); (b) Time-resolved DAP PL decay of Ga2O3 NCs in the NC conjugates having different CdSe/CdS to Ga2O3 NC concentration ratio, as indicated in the graph; (c) Quenching efficiency of the DAP PL of Ga2O3 NCs in the NC conjugate (squares) and with bound TGA (triangles).