Skip to main content
. 2016 Jun 14;6(6):115. doi: 10.3390/nano6060115

Figure 4.

Figure 4

Red squares: Development of PL intensity over the HA washing time for CdSe QDs synthesized in hexadecylamine/trioctylphosphine oxide (HDA/TOPO) (100:3:2, 30 min at 300 °C). Blue dots: Respective development of the hydrodynamic diameter together with the standard deviation for CdSe QDs measured by dynamic light scattering (DLS). For both, the half-life τ in min is given for the respective fitted exponential decay.