Skip to main content
. 2017 Feb 17;7:42816. doi: 10.1038/srep42816

Figure 7. Mineralisation of the extracellular matrix of hMSCs.

Figure 7

Mineralisation was determined by measuring the extracellular deposition of calcium in response to the treatment with 25(OH)D3 or 1α,25-(OH)2D3 at indicated concentrations during four weeks. Results are expressed as means ± SD (n = 2, *P < 0.05 and ***P < 0.001).