Skip to main content
. 2011 Apr 6;1(1):3–19. doi: 10.3390/nano1010003

Figure 5.

Figure 5.

(a) Photograph of a typical clay–CNT–chitosan fiber; (b, c) Scanning electron microscopy images of the fiber's surface morphology; (d) Typical fiber resistance as a function of time during exposure to humid atmosphere (21 °C, 90% RH) for 270 minutes.