Figure 1. Electrical characterization of the device in ethanol.

Figure 1

(a) Device capacitance (at 20 Hz) as a function of the water/EtOH concentration for different oxide thicknesses. (b) Capacitance as a function of frequency for different EtOH/water concentrations using a 15 nm-thick Al2O3-coated electrode. (c) The device equivalent circuit. The indexes ox, dl and sol correspond, respectively, to the capacitive and resistive contributions of the oxide, the electrical double layer and the solution bulk to measured impedance.