Group 1: SEM micrographs of the resins prepared with 150 % dilution using n-heptane/toluene as a diluent system at variable 2-vinyl pyridine/styrene/divinylbenzene ratios; (a) 30/4030;(b) 40/30/30 and (c) 50/20/30. Group 2: SEM micrographs of the resins synthesized with 100% dilution using n-heptane/ethyl acetate as a diluent system at 2-vinyl pyridine/styrene/divinylbenzene ratios; (a) 30/4030;(b) 40/30/30 and (c) 50/20/30. (Reprinted from [48], Copyright 2004, with permission from Elsevier).