Figure 3

CVs of 10 mM of PEG8–PDI in DMSO under N2 after adding incremental amounts of KO2 (20 μL of KO2 in DMSO, 0.0114 mM stock) containing of 0.1 M [(n-Bu)4N]ClO4 as a supporting electrolyte at 298 K with a glassy carbon working electrode and platinum wire as quasi-reference electrode. Scan rate: 50 mV/s. The arrow indicates the newly formed redox peak of the molecular O2. Color code: KO2 concentration increased from black to red.