Figure 8.

Figure 8

(a) CVs of PDI-1 under 1 atm O2 or Ar. All scans were collected at 100 mV s–1 using a GC working electrode with an area of 0.196 cm2. (b) LSV curves of RDEVs of PDI-1 in O2-saturated 0.1 M NaHPO4/NaH2PO4 buffer solution at pH 7 with different rotating speeds ranging from 400 to 1600 rpm. Inset: Koutecky–Levich plots of PDI-1 showing that n = 1.9. (c) RRDEV of PDI-1 in 0.1 M NaHPO4/NaH2PO4 buffer solution at pH 7 with a rotation speed 1600 rpm. The disk was scanned from 0.8 to −0.2 V while the ring electrode was held at 1.4 V. (d) The number of electrons transferred and the H2O2 yield of PDI-1during ORR as calculated by ring currents.