Table 1. Main physicochemical characterization for uncoated and CS-coated NPs.
Medium | MIL-100(Fe) | CS_MIL-100(Fe) | |
---|---|---|---|
BET surface area (m2g−1) | 1570 | 1590* | |
Size (nm) | Water | 135 ± 20 | 204 ± 32 |
PBS | 155 ± 61 | 182 ± 50 | |
lis-SIF | 147 ± 54 | 175 ± 30 | |
lis-SIF-panc | 168 ± 45 | 908 ± 36 | |
lis-SIF-muc | 254 ± 40 | 478 ± 85 | |
DMEM | 146 ± 37 | 273 ± 21 | |
HBSS | 163 ± 30 | 165 ± 5 | |
ζ-potential (mV) | Water | −18 ± 5 | +38 ± 5 |
PBS | −31 ± 0 | −28 ± 0 | |
lis-SIF | −51 ± 1 | −5 ± 3 | |
lis-SIF-panc | −7 ± 2 | −6 ± 3 | |
lis-SIF-muc | −6 ± 1 | −13 ± 9 | |
DMEM | −8 ± 2 | −24 ± 0 | |
HBSS | −18 ± 1 | +18 ± 2 |
For all media, both size and ζ-potential are measured in 5 min-aged suspensions to ensure comparable situations.
*BET surface area weight corrected by considering the presence of CS in the sample.