Skip to main content
. 2017 Mar 3;7:43202. doi: 10.1038/srep43202

Figure 9.

Figure 9

(ad) FESEM micrographs of the samples annealed at 1200 °C at different contents of zirconia; (a) x = 0.0, (b) x = 0.4, (c) x = 0.6, (d) x = 1.0.