Table 1. The crystallite size using different models: lattice strain, stress and the energy density of zirconia at x = 1.0 at different annealing temperatures.

T(°C) Ds (nm) UDM (nm) ε × 10−3 USDM (nm) UEDM (nm) Stress (MPa) U (kJ/m3)
1000 11.6 11.2 0.35 11.2 11.2 66.3 11.4
1100 17.4 15.4 −0.39 15.4 15.4 −74.4 14.4
1200 22.4 18.9 −2.78 18.9 18.9 −244.6 155.7
1300 56.6 39.6 −1.37 27.1 27.1 −263.8 181.1