Figure 2.

Figure 2

(a) reduction of structural quality in the case of photosensitized and pure SZ2080. Photoinitiator Irgacure 369 (IRG) containing cubes degrade slower and in a more progressive fashion. Conversely, the structures out of non-photosensitized material completely break up as soon as the fabrication parameters are not in the ΔI. All scales are 5 μm; and (b) monolithic micro-optical element on the tip of an optical fiber fabricated out of non-photosensitized SZ2080.