Scan Speed (mm∙s−1) Power (mW) 12 13 14 15
1 STABLE DAMAGED DAMAGED DAMAGED
2 STABLE DAMAGED DAMAGED DAMAGED
3 UNSTABLE STABLE STABLE DAMAGED
4 UNSTABLE STABLE STABLE STABLE
5 UNSTABLE STABLE STABLE STABLE
6 UNSTABLE UNSTABLE STABLE STABLE
7 Ø UNSTABLE STABLE STABLE
8 Ø UNSTABLE UNSTABLE UNSTABLE
9 Ø Ø UNSTABLE UNSTABLE
10 Ø Ø UNSTABLE UNSTABLE