Skip to main content
. 2017 Jan 18;10(1):76. doi: 10.3390/ma10010076

Figure 18.

Figure 18

Optical images of an AlSi10Mg alloy produced by means of DMLS and heat treated: (a) after a stress relieving at 300 °C for 2 h; (b) after a T4 treatment (c) after a T6 treatment (from the authors’ own unpublished work).