Skip to main content
. 2017 Mar 10;7:44144. doi: 10.1038/srep44144

Figure 10.

Figure 10

(a) STEM-HAADF micrograph of the same area shown in Fig. 5, the framed area is shown in greater detail in the TEM micrograph (b). The framed boundary between YS and Y-ZrO2 is again featured in greater detail (c) where the framed area is again presented in further detail (d).