Skip to main content
. 2017 Mar 16;172(4):15. doi: 10.1007/s00410-017-1329-1

Table 1.

EMP analyses of starting material glasses and experimental samples. The “halogen-free” glass was used as starting material for the synthesis of three “CMAS_start” glasses, which contain various amounts of H2O (Table 2) and halogens. These were used as starting materials for the partitioning experiments. Values represent the average of ten single measurements in the starting materials and five single measurements in each phase of each partitioning experiment. Uncertainties are given as 2σ. (b.d. = below detection limit). Crystal/melt ratios were determined via image analyses of BSE images using the software “ImageJ”

Sample SiO2 Al2O3 MgO CaO F Cl Total
Starting materials
Halogen-free 46.88 (51) 18.89 (33) 18.39 (26) 17.02 (31) b.d b.d 101.18 (95)
CMAS_start_dry 46.19 (57) 18.70 (44) 18.24 (19) 17.46 (30) 0.23 (4) 0.86 (2) 100.82 (118)
CMAS_start_05 45.74 (57) 18.56 (47) 17.87 (33) 17.36 (23) 0.27 (4) 0.58 (2) 99.80 (145)
 Sample SiO2 Al2O3 MgO CaO F Cl Total Crystal/melt
Partitioning experiments
Melt
 CMAS_dry 45.94 (62) 17.67 (22) 13.16 (30) 21.84 (41) 0.74 (4) 2.24 (12) 101.56 (100)
 CMAS_05 45.80 (88) 19.79 (33) 13.57 (38) 19.37 (62) 0.38 (6) 0.76 (6) 99.67 (156)
 CMAS_2 45.03 (86) 19.80 (50) 14.16 (24) 18.75 (43) 0.30 (4) 0.39 (4) 98.43 (153)
Olivine
 CMAS_dry 43.12 (68) b.d 57.69 (108) 0.58 (14) b.d b.d 101.39 (109) 0.12 (4)
 CMAS_05 42.84 (44) b.d 57.71 (71) 0.46 (3) b.d b.d 101.01 (98) 0.15 (5)
 CMAS_2 42.20 (41) 0.13 (10) 56.84 (85) 0.44 (8) b.d b.d 99.61 (127) 0.21 (4)
Anorthite
 CMAS_dry 43.67 (87) 35.69 (19) 0.28 (17) 19.84 (53) b.d b.d 99.84 (108) 0.34 (3)
 CMAS_05 43.58 (50) 35.81 (30) 0.30 (5) 19.79 (44) b.d b.d 99.48 (104) 0.06 (6)
Clinopyroxene
 CMAS_dry 52.09 (65) 6.22 (27) 18.09 (117) 24.06 (53) b.d b.d 100.46 (114) 0.04 (2)