Figure 4. Simultaneous SANS-DSC data for Pd41.25Ni41.25P17.5.

Figure 4

(a) The integrated detector counting rates as a function of temperature. The simultaneous DSC scan is superimposed, which shows a TC∼594 K at a heating rate of 2.5 K min−1. The coexistence of two phases can be clearly seen in the vicinity of TC. (b) Full-Q range SANS data for three samples: as-cast condition (C), quenched from 623 K after the transformation had ended (S1), and quenched after crystallization at 673 K (X). The nearly complete overlap of the SANS profiles between the as-cast and S1 samples demonstrates the reentrant behaviour.