(1) Galvanostatic charge-discharge cycles plotted against time(s) by use of an Ag/AgCl reference electrode, where the electrode consisting of graphite mixture as a working electrode and the electrode containing 30% Fe2O3 as a counter electrode; (a) counter electrode, (b) working electrode, and (c) cell potential. (2) Charge-discharge cycles for various symmetric and asymmetric capacitors containing Fe2O3, Fe3O4, V2O3, V2O5 and MnO2. The capacitors are expressed as positive electrode/negative electrode. (a) GA/Fe2 O3 (30%), (b) Fe2O3 (30%)/Fe2O3 (30%). (c) GA/Fe3O4 (30%), (d) Fe3O4 (30%)/Fe3O4(30%), (e) GA/V2O3 (30%), (f) GA/V2O5 (30%), (g) MnO2(30%)/GA(20%AC), (h) MnO2(30%)/Fe3O4(30%).